Skill and experience on the part of the craftsman are paramount for the process. Producing Celadon requires a great deal of time, care and concentration. The clay is first treated with additives which are then let in the shade and
thrown. After bisque firing at a temperature of 800 C, the glaze is
applied. The piece is then placed in the kiln for a second firing at a
temperature of 1,250 C, which gives the Celadon its inimitable, finely cracked
finish.
7 Moo 3, Chiang Mai-Sankampaeng Rd # 50130
315/1 Moo 5, Chiang Mai-Lampang Superhighway Chiang Mai 50140
116 Moo 5, Chiang Mai - Hod Rd. Chiang Mai 50230
-212 Moo 7, T.Narmphae, A. Hang Dong Chiang Mai 50230 -254 Moo 3, T. Baan Waen, A. Hang Dong Chiang Mai 50230
200 km.5 Chiang Mai-Hod Rd. Chiang Mai 50200
80/10 Soi Chom Doi, Canal Rd. Chiang Mai 50300
39 Moo4 Pa Tun Rd. Chiang Mai 50300
79/2 Arak Road Chiang Mai 50200
Moo1, T. Tasala Chiang Mai 50000
224 Moo 10, Chiang Mai Sankampaeng Rd. Chiang Mai 50130
60/3 Moo 10, Chiang Mai-Sankampaeng Rd. Chiang Mai 50130
Import Online - Buying Agent services ![]()
Content and design © 1997-2000 Chiang Mai-Online®, MCC Multitech, Co., Ltd. |